南京林业大学学报(自然科学版) ›› 2014, Vol. 38 ›› Issue (06): 115-120.doi: 10.3969/j.issn.1000-2006.2014.06.022

• 研究论文 • 上一篇    下一篇

竹束精细疏解与炭化处理对重组竹性能的影响

吴秉岭1,2,余养伦2,齐锦秋1,于文吉2*   

  1. 1.四川农业大学林学院,四川 雅安 625014;
    2.中国林业科学研究院木材工业研究所,国家林业局木材科学与 技术重点实验室,北京 100091
  • 出版日期:2014-12-31 发布日期:2014-12-31
  • 基金资助:
    收稿日期:2013-11-20 修回日期:2014-01-28
    基金项目:浙江省省院合作林业科技重大项目(2011SY01); 国家自然科学基金面上项目(31070494)
    第一作者:吴秉岭,硕士生。*通信作者:于文吉,研究员。E-mail:yuwenji@caf.ac.cn。
    引文格式:吴秉岭,余养伦,齐锦秋,等. 竹束精细疏解与炭化处理对重组竹性能的影响[J]. 南京林业大学学报:自然科学版,2014,38(6):115-120.

Effects of bamboo bundles treated with fine fluffing and carbonized treatment on the properties of bamboo scrimber

WU Bingling1,2, YU Yanglun2, QI Jinqiu1, YU Wenji2*   

  1. 1. College of Forestry, Sichuan Agricultural University, Ya'an 625014, China;
    2. Research Institute of Wood Industry,Chinese Academy of Forestry, Key Laboratory of Wood Science and Technology of State Forestry Administration,Beijing 100091,China
  • Online:2014-12-31 Published:2014-12-31

摘要: 以去青留黄的竹片为原料,利用纤维原位可控分离技术,对竹片进行精细化疏解处理,再经浸胶、干燥后,采用热压法制备重组竹,并与普通的本色重组竹、低温炭化重组竹、高温炭化重组竹以及竹基纤维复合材料进行对比。结果表明:高温热处理是提高重组竹的耐水性能和尺寸稳定性的有效方法之一,其缺点是力学性能损失严重,静曲强度损失率达到45%; 与高温炭化处理相比,精细疏解加工工艺简单,加工的重组竹力学性能基本不损失,且能更有效地改善重组竹的耐水性能和尺寸稳定性; 与普通本色重组竹相比,采用精细化疏解竹束制备的重组竹,其吸水率降低75%,吸水厚度膨胀率降低67%,耐水性能和尺寸稳定性接近竹基纤维复合材料。

Abstract: This study explored novel bamboo scrimber fabricated using fine fiber bundles and phenolic resins via hot-pressing process. The mechanical properties, water resistance and dimensional stability of novel bamboo scrimber were investigated, and the results were compared with commercial bamboo scrimber made from control and carbonized bamboo bundles and bamboo-based fiber composites. The results showed that fine fluffing treatment and high temperature thermal treatment showed good technological properties with improved water absorption and dimensional stability. However, the mechanical properties of bamboo scrimber were obviously decreased by high-temperature thermal treatment with 45% decrease of MOR comparing with that of control. The fine fluffing treatment would improve bamboo scrimber dimensional stability while maintains its mechanical properties with 67% decrease of thickness swelling and 75% decrease of water absorption comparing with that of control. The water resistance and dimensional stability of bamboo scrimber made from bamboo bundles with fine fluffing was close to that of the bamboo-based fiber composites.