<正>结合多年的施工经验,从材料选用、配合比设计、铺筑方法等方面分析二灰碎石基层施工中的质量控制措施。结果表明:在摊铺作业时,应保持作业的连续性;在气温较高时施工,应保证碾压时二灰碎石的含水量,并快速摊铺、碾压;施工完毕要保湿养生7d,气温较低时还需采取覆盖措施,防止表面冻坏。

Abstract

The measures for controlling construction quality of lime-fly bound macadam base of pavement were studied from the respects of selecting materials, designing mix proportion and paving methods. The results as follows: the work would be continuous on spreading. In- conditions of high temperature, the moisture content of lime-fly ash bound macadam would be keeped on rolled work doing, and spreading and rolled work would be quick. After rolled work, maintenance would be kept with moisture within 7 days, in conditions of low tempera- ture, road would be covered with material to prevent it frozen.

引用本文

导出引用
穆传刚,史建华. 二灰碎石基层施工质量的控制措施[J]. 南京林业大学学报(自然科学版). 2006, 30(S1): 58-60 https://doi.org/10.3969/j.jssn.1000-2006.2006.07.017
MU Chuan-gang,SHI Jian-hua. Measures for Controlling Construction Quality of Lime-fly Bound Macadam Base of Pavement[J]. JOURNAL OF NANJING FORESTRY UNIVERSITY. 2006, 30(S1): 58-60 https://doi.org/10.3969/j.jssn.1000-2006.2006.07.017
中图分类号: U416.1   

Accesses

Citation

Detail

段落导航
相关文章

/